Follow
Giuseppe Pintaude
Title
Cited by
Cited by
Year
The use of a Vickers indenter in depth sensing indentation for measuring elastic modulus and Vickers hardness
AR Franco Jr, G Pintaúde, A Sinatora, CE Pinedo, AP Tschiptschin
Materials Research 7, 483-491, 2004
1242004
An approach to elucidate the different response of PVD coatings in different tribological tests
JCA Batista, C Godoy, G Pintaúde, A Sinatora, A Matthews
Surface and Coatings Technology 174, 891-898, 2003
722003
Introduction of the Ratio of the Hardness to the Reduced Elastic Modulus for Abrasion
G Pintaude
Tribology - Fundamentals and Advancements, 217-230, 2013
69*2013
Mild and severe wear of steels and cast irons in sliding abrasion
G Pintaude, FG Bernardes, MM Santos, A Sinatora, E Albertin
Wear 267 (1-4), 19-25, 2009
612009
The effects of abrasive particle size on the sliding friction coefficient of steel using a spiral pin-on-disk apparatus
G Pintaude, DK Tanaka, A Sinatora
Wear 255 (1-6), 55-59, 2003
532003
Uncertainty analysis on the wear coefficient of Archard model
CRÁ da Silva Jr, G Pintaude
Tribology International 41 (6), 473-481, 2008
482008
The particle size effect on abrasive wear of high-chromium white cast iron mill balls
G Pintaude, AP Tschiptschin, DK Tanaka, A Sinatora
Wear 250 (1-12), 66-70, 2001
462001
Effect of tool geometry on the wear of cemented carbide coated with TiAlN during drilling of compacted graphite iron
VV De Oliveira, PAC Beltrão, G Pintaude
Wear 271 (9-10), 2561-2569, 2011
382011
Abrasion and corrosion resistance of new Ni–based coating deposited by HVOF thermal spray process
M Benegra, M Magnani, H Goldenstein, O Maranho, G Pintaude
Surface Engineering, 2010
342010
Effect of specimen preparation on contact fatigue wear resistance of austempered ductile cast iron
C Brunetti, MV Leite, G Pintaude
Wear 263 (1-6), 663-668, 2007
302007
Scratch resistance of low-temperature plasma nitrided and carburized martensitic stainless steel
AC Rovani, R Breganon, GS de Souza, SF Brunatto, G Pintaúde
Wear 376, 70-76, 2017
292017
Análise dos regimes moderado e severo de desgaste abrasivo utilizando ensaios instrumentados de dureza
G Pintaúde
Escola Politécnica da USP, Departamento de Engenharia Mecânica, Sao Paulo, 2002
24*2002
Investigations on quality characteristics in gas tungsten arc welding process using artificial neural network integrated with genetic algorithm
IV Tomaz, FHG Colaço, S Sarfraz, DY Pimenov, MK Gupta, G Pintaude
The International Journal of Advanced Manufacturing Technology 113 (11 …, 2021
222021
Relación entre factores micro-estructurales e impacto repetido en aleaciones de alto cromo para bolas de molino.//Relationship among factors micro-structural and impact …
E Albertin, A Sinatora, G Pitaluga, A Parada
Ingeniería Mecánica 11 (1), 57-62, 2008
222008
Identification of abrasion regimes based on mechanisms of wear on the steel stylus used in the Cerchar abrasiveness test
GR Piazzetta, LE Lagoeiro, IFR Figueira, MAG Rabelo, G Pintaude
Wear 410, 181-189, 2018
172018
Wear and Corrosion Resistances of Active Screen Plasma-Nitrided Duplex Stainless Steels
G Pintaude, AC Rovani, JCK das Neves, LE Lagoeiro, X Li, HS Dong
Journal of Materials Engineering and Performance 28 (6), 3673–3682, 2019
162019
Influence of Fe on the room and high-temperature sliding wear of NiAl coatings
C Brunetti, LP Belotti, MH Miyoshi, G Pintaude, A D’Oliveira
Surface and Coatings Technology 258, 160-167, 2014
162014
Comparison of scratch resistance of lamellar and compacted graphite irons used in cylinder liners
JL do Vale, M Cortz, VMS Bertolini, CH da Silva, G Pintaude
Journal of the Brazilian Society of Mechanical Sciences and Engineering, 1-8, 2017
152017
Characteristics of Abrasive Particles and Their Implications on Wear
G Pintaude
New Tribological Ways, 117-130, 2011
152011
Effect of indentation size and microhardness calculation on abrasive wear severity
G Pintaude, DK Tanaka, A Sinatora
Scripta Materialia 44 (4), 659-663, 2001
152001
The system can't perform the operation now. Try again later.
Articles 1–20